Xapa de placa d'acer inoxidable ASTM A240 904L DIN1.4539 X1NiCrMoCuN25-20-5

Feb 24, 2026

Deixa un missatge

Stainless Steel Grade 904L - Super Austenitic Anti-CorrosionHow to Buy 904L Stainless Steel Sheet from Reliable Suppliers?What is SAE 904L stainless steel sheet?

Descripció del producte

Grade 904L stainless steel is a non-stabilized austenitic stainless steel with low carbon content. This high alloy stainless steel is added with copper to improve its resistance to strong reducing acids, such as sulphuric acid. The steel is also resistant to stress corrosion cracking and crevice corrosion. Grade 904L is non-magnetic, and offers excellent formability, toughness and weldability.

El grau 904L conté grans quantitats d'ingredients cars, com ara molibdè i níquel. Avui en dia, la majoria de les aplicacions que utilitzen el grau 904L se substitueixen per acer inoxidable dúplex de baix cost-2205.

Propietats clau

Les seccions següents descriuen les propietats dels productes laminats plans a ASTM B625. És possible que les especificacions no siguin idèntiques per a altres productes com ara barres, tubs i canonades.

Composició

La taula següent proporciona els rangs de composició dels acers inoxidables de grau 904L:

Taula 1. Intervals de composició dels acers inoxidables de grau 904L

Grau C Mn Si P S Cr Mo Ni Cu
904L

min.

màx.

-

0.02

-

2

-

1

-

0.045

-

0.035

19

23

4

5

23

28

1

2

Propietats mecàniques

Les propietats mecàniques típiques dels acers inoxidables de grau 904L es mostren a la taula següent:

Taula 2. Propietats mecàniques dels acers inoxidables de grau 904L

Grau Resistència a la tracció (MPa) min Límit de rendiment 0,2% Prova (MPa) min Elongació (% en 50 mm) min Duresa
Rockwell B (HR B) Brinell (HB)
904L 490 220 36 70-90 típic 150

 

Enviar la consulta